The Influence Of Repair Welded Joint On The Life Of Steam Pipeline Made Of Cr-Mo Steel Serviced Beyond The Calculated Working Time

Open access

Abstract

The aim of the paper was to examine the influence of repair welded joints on the service life of steam pipelines for over 220 000 hours of service in creep conditions. The research included the study of the microstructure using scanning microscopy, the tests on mechanical properties at room and elevated temperature, determining the nil ductility transition temperature, and short-time creep tests to determine the residual life of the material. The tests allowed determining the time of further safe operation of elements of the steam pipeline with a repair welded joint, with reference to the base material, and the welded joint after service. The assessment of residual life and disposable residual life, and at the same time determining the possible time of further safe operation, has an essential meaning in the case of elements serviced considerably beyond the calculated working time.

[1] J. Dobrzański, Materials science interpretation of the life of steels for power plants. Open Access Library, (2011).

[2] A. Zieliński, J. Dobrzański, D. Renowicz, A. Hernas, Fifth International Conference on Advances in Material Technology for Fossil Power Plants, 34, (2007).

[3] J. Dobrzański, A. Zieliński, H. Krztoń, J. of Achiev. Mater. Manufact. Eng. 23, 39 (2007).

[4] J. Dobrzański, H. Krztoń, A. Zieliński, J. of Achiev. Mater. Manufact. Eng. 23, 19 (2007).

[5] J. Dobrzański, Journal of Mater. Proc. Techn. 157-158, 297 (2004).

[6] G. Bakic, V. Sijacki Zeravcic, M. Djukic, V. Maksimovic, B. Rajicic, (2013, May) First Metallurgical & Materials Engineering Congress of South-East Europe (MME SEE 2013), Belgrade, Serbia, 380 (2013).

[7] K. Kubushiro, N. Saito, H. Nakagawa, K. Sawada, K. Kimura, ASME 2014 Pressure Vessels and Piping Conference, V06AT06A044 (2014).

[8] X.W. Zhu, H.H. Cheng, M.H. Shen, J.P. Pan, J.P. Advan. Mater. Res. 791, 382 (2013).

[9] I.I. Mintz, L.E. Khodykina, Thermal Eng. 60, 444 (2013).

[10] A. Zieliński, J. Dobrzański, Prace IMŻ 3, 42 (2013). (in Polish)

[11] A. Zieliński, J. Dobrzański, M. Dziuba-Kałuża, Archiv. Mater. Sc. Eng. 61, 69 (2013).

[12] O.Z. Student, L.M. Svirs’ka, I.R. Dzioba, Mater. Sc. 48, 239 (2012).

[13] J. Dobrzański, H. Paszkowska, A. Zieliński, 9th Liege Conference on Materials for Advanced Power Engineering, 400 (2010).

[14] P. Parameswaran, K. Laha, K.S. Chandravathi, K. Bhanu Sankaro Rao, Trans. Indian Institute Metals. 63, 479 (2010).

[15] PN-75/H-84024 Steels for elevated temperatures service. Grades.

[16] M. Dziuba-Kałuża, J. Dobrzański, A. Zieliński, Prace IMŻ 65, 64 (2013). (in Polish)

Archives of Metallurgy and Materials

The Journal of Institute of Metallurgy and Materials Science and Commitee on Metallurgy of Polish Academy of Sciences

Journal Information


IMPACT FACTOR 2016: 0.571
5-year IMPACT FACTOR: 0.776

CiteScore 2016: 0.85

SCImago Journal Rank (SJR) 2016: 0.347
Source Normalized Impact per Paper (SNIP) 2016: 0.740

Cited By

Metrics

All Time Past Year Past 30 Days
Abstract Views 0 0 0
Full Text Views 218 155 8
PDF Downloads 86 65 5